1050 / C50 / S50C
1050 steel is a medium-carbon steel offering good strength, hardness and wear resistance. It can be heat treated to achieve higher mechanical strength and is suitable for components requiring improved surface hardness through induction or flame hardening.
Available Form
Round Bar
Custom Diameter & Length
Flat Bar
Custom Thickness, Width & Length
Square Bar
Custom Width & Length
Steel Plate
Custom Thickness, Width & Length
Steel Grade Comparison
| W-Nr | EN | AISI | JIS |
| 1.1213 | CK50 | 1050 | S50C |
Chemical Composition(wt%)
| C | Mn | P | S | Fe |
| 0.48~0.55 | 0.60~0.90 | ≤0.04 | ≤0.05 | Balance |
Physical Properties
Density:7.85 g/cm³
Modulus of Elasticity: 200 GPa
Thermal Conductivity: 49.8 W/(m.K) at 100°C
| Temperature | 20-100°C | 2-200°C | 2-300°C | 2-400°C |
| Coefficient of Thermal Expansion (×10-6 /K) | 12.0 | – | – | 13.5 |
Heat Treatment Process
Hardening: Heat evenly to 820–860°C, then quench in water or oil.
Annealing: Heat the steel evenly to 680–710°C, hold until uniform, then cool slowly inside the furnace.
Tempering: Heat uniformly to 550–660°C, hold, and cool in still air. Typical hardness: 20–30 HRC (depending on tempering temperature).