S7 | 1.2357

S7 is an air-hardening shock-resisting tool steel offering excellent toughness, high impact resistance, and good hardenability. It also provides good resistance to softening at elevated temperatures, making it suitable for tools and dies exposed to repeated impact and heavy loading.
Available Form
Round Bar
Custom Diameter & Length
Flat Bar
Custom Thickness, Width & Length
Square Bar
Custom Width & Length
Steel Plate
Custom Thickness, Width & Length
Steel Grade Comparison
W-Nr EN AISI JIS
1.2357 50CrMoV13-14 S7 –
Chemical Composition(wt%)
C Si Mn Cr Mo V
0.45~0.55 0.20~1.00 0.20~0.80 3.00~3.50 1.30~1.80 ≤0.35
Physical Properties

Density:7.86 g/cm³
Modulus of Elasticity: 207 GPa
Thermal Conductivity: 28.0 W/(m.K)

Temperature 20-100°C 2-200°C 2-300°C 2-400°C
Coefficient of Thermal Expansion (×10-6 /K) 11.7 12.9 13.3 13.8
Heat Treatment Process

Hardening: Heat the steel evenly to 925-955°C until the whole section reaches temperature. Then quench in oil and air to cool.
Annealing: Heat the steel to 815-845°C, hold it well at temperature, and then let it cool slowly inside the furnace.
Tempering: Heat the steel uniformly, hold it at the selected tempering temperature, and then allow it to cool in still air. tempering temperature 205~620°C, hardness 57~45HRC

Application Fields
Chisels, punches, rivet sets, and driver bolts. shear blades and cutting tools exposed to impact. blanking, bending, and forming dies. hot punching, shearing, and selected extrusion dies. zinc die-casting dies and related tooling. mold components requiring high toughness and impact resistance.
Disclaimer: the information and data presented herein are typical values for reference and are not intended as warranties to readers.