8418 | 1.2367
1.2367 (X38CrMoV5-3) is a hot work tool steel offering excellent high-temperature strength, tempering resistance, and good toughness. It provides high wear resistance and good hardenability, making it suitable for demanding forging, die casting, and hot extrusion applications.
Available Form
Round Bar
Custom Diameter & Length
Flat Bar
Custom Thickness, Width & Length
Square Bar
Custom Width & Length
Steel Plate
Custom Thickness, Width & Length
Steel Grade Comparison
| W-Nr | EN | AISI | JIS |
| 1.2367 | X38CrMoV5-3 | – | – |
Chemical Composition(wt%)
| C | Si | Mn | P | S | Cr | Mo | V |
| 0.35~0.40 | 0.30~0.50 | 0.30~0.50 | P≤0. 03 | 0. 02 | 4. 80~5. 20 | 2. 70~3. 20 | O. 40~0.60 |
Physical Properties
Density:7.83 g/cm³
Thermal Conductivity: 25.0 W/(m.K)
| Temperature | 20-100°C | 2-200°C | 2-300°C | 2-400°C |
| Coefficient of Thermal Expansion (×10-6 /K) | 11.5 | 12.0 | 12.2 | 12.5 |
Heat Treatment Process
Hardening: Heat the steel evenly to 1030-1050°C until the whole section reaches temperature. Then quench in oil to cool.
Annealing: Heat the steel to 800-840°C, hold it well at temperature, and then let it cool slowly inside the furnace.
Tempering: Heat the steel uniformly, hold it at the selected tempering temperature, and then allow it to cool in still air.
| Tempering Temperature | 400°C | 500°C | 600°C | 650°C |
| Hardness (HRC) | 53 | 54 | 52 | 46 |
Application Fields
Wear resisting tools, pressure die casting tools, pressing tools for light and heavy metal.
Disclaimer: the information and data presented herein are typical values for reference and are not intended as warranties to readers.